Customization: | Available |
---|---|
After-sales Service: | 1 Year |
Warranty: | 1 Year |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Hot Sell PVC WPC Door Panel Extrusion Production Line Wood Plastic Composite Foam Board Making Machine Price
This production line is consisted by following parts:
1. The conical screw extruder keep a high output for the extrusion
2. T-die make the processing evenly (thickness is adjustable)
3. Shaping mould keep a good shape and high precision of the finished PVC foamed board
4. Cooling trial with two side blade cutting for the thinner sheet
5. Laminating device
6. Haul-off device with normal 8 rubber roller groups and two side saw cutting for thicker board
7. The auto saw cutter the dust collection device
8. Stacker
Advantage and application:
1 the excellent appearance of the natural wood,
2 With the advantages of anti-corrosion, moisture-proof, anti-moth-eaten, dimensional-steady, no cracking, etc, it is much harder than the pure plastic products and has the similar process-ability as the wood.
3 It can be cut, paint, bonded and fixed with nails or bolts.
4 The PVCfoamed board is mainly used in wall panel, decorating plate, construction formwork, kitchen cabinet, cloth cabinet, bath room cabinet, fence, stair handrail, etc.
Type |
PVC Free foamed board |
PVC skinning foamed board |
WPC/PVC muti-layer co-extrusion fomed board |
Model |
SJZS80/SJZS92 twin screw extruder |
SJZS80/SJZS92 twin screw extruder |
SJZS80+SJZS65 SJZS92+SJZS65 twin screw extruder |
Board width (mm) |
600-1220mm |
600-1220mm |
600-1220mm |
Thicknessm (mm) |
3-25mm |
3-25mm |
3-25mm |
Main motor (kw) |
75kw/110kw |
75kw/110kw |
75kw+37kw/110kw+37kw |
1,Q:How to solve the problem about material leakage of high mixer quickly?
A:Replace the seal gasket or check the cylinder distance whether it is enough .
2,Q:why the low-mixer is always burned?
A:The mixture exceeds the rated capacity, causing the motor to overload.
3,Q:How to adjust the space of the screw?
A:Log in Polytech official website, authorized to download the video tutorial.
4,Q:How to solve the the ASA coating problem?
A:Many reasons ,such as temperature, formulation, start-up speed etc.
5,Q:Why the material Burnt?
A:Many reasons, such as high heating temperature, heating preservation time is too long.
6, Q:Why the ASA is covering on the bottom?
A:Many reasons ,such as temperature, formulation, start-up speed does not match.
7, Q:Asymmetrical ASA2/4 area covering?
A:Many reasons ,such as temperature, formulation, start-up speed does not match.
8,Q:How to adjust the dislocation of glazed tile module?
A:By adjusting tooth on the dynamic column to achieve the right location of module.
9, Q:Why Shaping mould two side speed is not synchronization?
A:Two side shaping module is not synchronized.
10,Q:Why the Cutter machine does not move?
A:Replace the sliding bearing seat under rack or moving cylinder.